**Author:** ![Roger\_Irwin](https://avatars.discourse-cdn.com/v4/letter/r/ecd19e/32.png) [@Roger\_Irwin](https://forum.clcboats.com/u/Roger_Irwin)\
**Post date:** [December 28, 2014, 11:37pm UTC](https://forum.clcboats.com/t/newbie-issue/42759/1 "2014-12-28T23:37:22Z")

</div>

I am building a Passagemaker take-apart. &nbsp; Woodworking and epoxy stitch building is all new to me. &nbsp;I decided to use Peel Ply to ensure a bubble free and smooth finish. &nbsp;In general I'm getting getting GREAT results except where the Peel-Ply material was folded for shipment. &nbsp;The Peel-Ply then leaves either depressions in the epoxy or ridges along the crease fold. &nbsp; &nbsp;I've tried smoothing out the material to no avail - can I iron out the creases with a clothes iron or spray water on the peel ply to eliminate the fabric creases? &nbsp;I believe I recall that peel-ply has a special "epoxy release" treatment so I dont want to damage the release properties while trying to get rid of the devilish creases. &nbsp; Thanks!!

&nbsp;

&nbsp;

&nbsp;

---

<div class="post-metadata">

**Author:** ![Roger\_Irwin](https://avatars.discourse-cdn.com/v4/letter/r/ecd19e/32.png) [@Roger\_Irwin](https://forum.clcboats.com/u/Roger_Irwin)\
**Post date:** [January 12, 2015, 3:06pm UTC](https://forum.clcboats.com/t/newbie-issue/42759/2 "2015-01-12T15:06:19Z")

</div>

&nbsp; &nbsp;I contacted WestEpoxy and spoke to their technical reps about the creases in the Peel-Ply telegraphing into the epoxy and thus leaving valleys or ridges in the epoxy. &nbsp;

He suggested a heat gun on the material to relax the material and eliminate the creases. &nbsp; &nbsp;I tried my wifes hair dryer on hot with very minor improvements. &nbsp; However ironing the material works magically if done on both sides of the material. &nbsp; I then roll the material up on a cardboard tube to prevent new creases. &nbsp;Major improvement with no touch-up required afterwards and the surface does not need to be sanded for the next coat. &nbsp;&nbsp;

&nbsp;

---

<div class="post-metadata">

**Author:** ![Sullivan\_Bradley](https://avatars.discourse-cdn.com/v4/letter/s/a698b9/32.png) [@Sullivan\_Bradley](https://forum.clcboats.com/u/Sullivan_Bradley)\
**Post date:** [January 12, 2015, 5:07pm UTC](https://forum.clcboats.com/t/newbie-issue/42759/3 "2015-01-12T17:07:32Z")

</div>

&nbsp; &nbsp;Roger, I'm curious about the types of surfaces you're successfully using Peel-Ply on. In the CLC shop tips section, it says that the technique works well on flat surfaces (they use a hatch panel as a suitable surface) but not so good on the curved surfaces. Are you finding that Peel-Ply is working on the hull panels or other curving surfaces? Thanks.&nbsp;

---

<div class="post-metadata">

**Author:** ![Roger\_Irwin](https://avatars.discourse-cdn.com/v4/letter/r/ecd19e/32.png) [@Roger\_Irwin](https://forum.clcboats.com/u/Roger_Irwin)\
**Post date:** [January 12, 2015, 10:15pm UTC](https://forum.clcboats.com/t/newbie-issue/42759/4 "2015-01-12T22:15:20Z")

</div>

&nbsp; &nbsp;The CLC shop tips section is 100% correct for compound curves. &nbsp;So curves in 2 dimensions. &nbsp; By way of example a saddle shape would be a compound curve. &nbsp;Deck surfaces that curve both bow to stern and port to starboard would also be a compound curve. &nbsp;For such cases the peel ply would pucker and the underlying epoxy would have large ripples or ridges of epoxy or worse that would need fairingor major rework. Simply -trying to use peel ply on compound curves would be a dogs breakfast mess. &nbsp; &nbsp;In my use case, I am applying peel ply on flat Okoume plywood so strakes, bulkheads, transoms and seating surfaces directly after the first coat. &nbsp;After smoothing with a plastic squeegee(sp?) this yields a dead flat surface without epoxy bubbles without hillocks or bumps that requires no sanding for the 2nd coat. &nbsp;My target for the PMD is to do 2 epoxy coats for all the pieces prior to stitching it together. &nbsp;&nbsp;

Personally I see no reason why peel ply would not work well for a simple curve such as a tube shape where the curve is only changing in one dimension, or a hatch cover with a curve only in one direction say port to starboard, but this is all new to me. &nbsp;

&nbsp;