**Author:** ![Brian\_Klaver](https://avatars.discourse-cdn.com/v4/letter/b/ac8455/32.png) [@Brian\_Klaver](https://forum.clcboats.com/u/Brian_Klaver)\
**Post date:** [February 3, 2012, 9:08am UTC](https://forum.clcboats.com/t/switching-for-mas-to-west-system/39297/1 "2012-02-03T09:08:28Z")

</div>

I am concerned about running out of epoxy on my build but so far I am not sure if it will happen or not.&nbsp;&nbsp; In calling around town, there is nobody around here that is selling the Mas epoxy I am currently using.&nbsp;&nbsp; If I do need to purchase some to finish to the job can I switch to West System brand or can you not put different products over top one another?

I know I can order it online and wait for it....just wondering if one day I am in a bind and need to go pick some up, can I go with West?

---

<div class="post-metadata">

**Author:** ![jbt](https://avatars.discourse-cdn.com/v4/letter/j/6bbea6/32.png) [@jbt](https://forum.clcboats.com/u/jbt)\
**Post date:** [February 3, 2012, 1:19pm UTC](https://forum.clcboats.com/t/switching-for-mas-to-west-system/39297/2 "2012-02-03T13:19:02Z")

</div>

Klaver,

I did just that on my Northeaster Dory (used it on the skeg and the skeg filet). No problems. The West seems to be a little less hard when fully cured than the MAS, but it painted just like the MAS.

Good luck.

JB

---

<div class="post-metadata">

**Author:** ![Brian\_Klaver](https://avatars.discourse-cdn.com/v4/letter/b/ac8455/32.png) [@Brian\_Klaver](https://forum.clcboats.com/u/Brian_Klaver)\
**Post date:** [February 3, 2012, 1:45pm UTC](https://forum.clcboats.com/t/switching-for-mas-to-west-system/39297/3 "2012-02-03T13:45:36Z")

</div>

Did it sand out just as well as the MAS?&nbsp;&nbsp; If I run out I suspect it will be on the top and I was just trying to determine if it is worth mail ordering the Mas or if they really just aren't that different.&nbsp;&nbsp; One product is available 10 minutes from my house and the other I have to order a wait for so I was hoping the West System stuff worked fine and could go over existing Mas stuff with no issues.&nbsp;&nbsp;

---

<div class="post-metadata">

**Author:** ![David\_Bartnowski](https://avatars.discourse-cdn.com/v4/letter/d/dec6dc/32.png) [@David\_Bartnowski](https://forum.clcboats.com/u/David_Bartnowski)\
**Post date:** [February 3, 2012, 6:23pm UTC](https://forum.clcboats.com/t/switching-for-mas-to-west-system/39297/4 "2012-02-03T18:23:56Z")

</div>

I have used a lot of West Epoxy, for both wood projects and glass projects. &nbsp;I am now a MAS believer. &nbsp;One thing about the West Epoxy is you will have to get their special hardner that is clear, otherwise, you will be getting a more amber color. &nbsp;I will be short epoxy for my Shearwater Sport hybrid, and will use some West for the end pours, but will be ordering more MAS for the final coat. &nbsp;I have almost enough MAS, or might make it, but don't want to take a chance.

---

<div class="post-metadata">

**Author:** ![Scott\_Denning](https://avatars.discourse-cdn.com/v4/letter/s/67e7ee/32.png) [@Scott\_Denning](https://forum.clcboats.com/u/Scott_Denning)\
**Post date:** [March 14, 2012, 11:55pm UTC](https://forum.clcboats.com/t/switching-for-mas-to-west-system/39297/5 "2012-03-14T23:55:31Z")

</div>

After setting for a couple months, I used MAS and the epoxy failed to fully cure.&nbsp; I cleaned the pumps with white vinegar and tried again, it cured perfectly.&nbsp; Evidently the pumps were gummed up a little and weren't metering correctly after setting for a couple months.&nbsp; Before the next build, I'll clean the pumps again or use new pumps.

I still have some WEST resin and fast hardener, I'll be using it up on scarfs and other connections that I want to be able to stress after a short cure period.

Scott Denning  
Huntington WV

---

<div class="post-metadata">

**Author:** ![Paul\_Faulkner](https://avatars.discourse-cdn.com/v4/letter/p/f17d59/32.png) [@Paul\_Faulkner](https://forum.clcboats.com/u/Paul_Faulkner)\
**Post date:** [March 15, 2012, 1:32pm UTC](https://forum.clcboats.com/t/switching-for-mas-to-west-system/39297/6 "2012-03-15T13:32:09Z")

</div>

I used West to build a dinghy and MAS to build 2 kayaks.&nbsp; I much prefer the MAS.&nbsp; The West will blush.&nbsp; Ditto what dave10990 said about the amber color.&nbsp; I had some West laying around, so I used it for my end pours.&nbsp; I would not use it on any visible areas.

Paul in Phoenix

&nbsp;