I have some older MAS resin (3 years?) that has clumped up in the bottle. I am seeing on the web that a warm water bath will restore it to workable condition?
john
I have some older MAS resin (3 years?) that has clumped up in the bottle. I am seeing on the web that a warm water bath will restore it to workable condition?
john
Not sure I understand the question. Yes, lumpy (or crystallized) resin will be restored good as new by a warm water bath. No need to replace it. The warmer the water the better (within reason). I like about 140 Fahrenheit.
Have fun,
Laszlo
Thanks Lazlo,
Yes - that was the question. I was confirming with this group that heating crystalized resin will restore it. Phew!
John
I used to know a guy named Lumpy Resin. He was in hot water all the time....